Today polished iron foils were mounted to two pucks, a) 1006 steel fabricated for GTS gun and b) molybdenum fabricated for bench tests. Both pucks were heated in dry nitrogen glove box with a small square of indium foil on top. At about 300C the indium foil melts and the iron foils are placed and centered. The pucks are moved off the heater and allowed to cool. Later, tantalum retaining rings with ID 11mm were press fit and crimped to the pucks.

Here are some picks:

File:IMG 4183.JPG File:IMG 4184.JPG File:IMG 4185.JPG File:IMG 4186.JPG File:IMG 4187.JPG