Updates

  • Cathode front end piece fabrication
    • Drawings for option A (16/30 deg) and option B (16/60 deg) have been finalized and submitted to the machine shop
    • Matt Poelker provided 316 L Vacuum Arc Re-melt Stainless Steel. Carlos delivered this material to Vince. Carlos to check with Matt supply chain.
    • Cathode front end 16-30 test piece was polished using the tumbler barrel. Machining marks on the cone were not fully removed, but piece looks very well polished on the rim.
    • This test piece was dry fitted to a spare ball electrode. This piece fits very well as expected.