Difference between revisions of "Mar 13 2024"

From Ciswikidb
Jump to navigation Jump to search
(Created page with "==Updates== * Cathode front end piece fabrication ** Drawings for option A (16/30 deg) and option B (16/60 deg) have been finalized and submitted to the machine shop ** Matt...")
 
Line 6: Line 6:
 
** Cathode front end 16-30 test piece was polished using the tumbler barrel. Machining marks on the cone were not fully removed, but piece looks very well polished on the rim.
 
** Cathode front end 16-30 test piece was polished using the tumbler barrel. Machining marks on the cone were not fully removed, but piece looks very well polished on the rim.
 
** This test piece was dry fitted to a spare ball electrode. This piece fits very well as expected.
 
** This test piece was dry fitted to a spare ball electrode. This piece fits very well as expected.
 +
** [[File:Sample cathode front end piece on sample ball pic02.jpg|right|middle|thumb]]

Revision as of 16:17, 26 March 2024

Updates

  • Cathode front end piece fabrication
    • Drawings for option A (16/30 deg) and option B (16/60 deg) have been finalized and submitted to the machine shop
    • Matt Poelker provided 316 L Vacuum Arc Re-melt Stainless Steel. Carlos delivered this material to Vince. Carlos to check with Matt supply chain.
    • Cathode front end 16-30 test piece was polished using the tumbler barrel. Machining marks on the cone were not fully removed, but piece looks very well polished on the rim.
    • This test piece was dry fitted to a spare ball electrode. This piece fits very well as expected.
    • Sample cathode front end piece on sample ball pic02.jpg